Kenplas Forum ==> Injection Molding (Machine) ==> Preform Body Opaque/Haze
<< Previous Topic Next Topic >>
1

1. PET resin should be properly dried or dehumidified (drying temperature, duration);
2. Increase barrel temperature setting;
3. Increase RPM in case plasticization is insufficient;
4. Enhance cooling water for mold (Post crystallinity decrease melt temperature).

Fine
5
Poor
1
2006-2-15 11:20:14 By Kenplas