SIR,
CAN ANY ONE SUGGEST A RIGHT DESIGN OF SCREW FOR SOLUTION OF OUR PROBLEM?

WE PROCESS 0.30 MFI HDPE MATERIAL TO MAKE PE PREFORMS (WHICH IS BLOWN INSINGLE STAGE IBM M/c) WT. RANGING 60g ~ 100g ON A IBM M/c HAVING 45 Dia. SCREW & 160 + 10 mm STROKE.

WE R FACING A PROBLEM OF GENERATING OF BLACK & BROWN SPECS RANDOMLY AFTER FEW WEEKS.

ON INCREASING A COMPRESSION RATIO FROM 1.35 TO 1.6, IT WAAS REDUCED TO 40% BUT ANOTHER QUALITY RELATED PROBLEMS LIKE BLACK LINE ALONG P[ARTING LINE HAS BEEN STARTED.

Fine
2
Poor
2009-5-2 13:59:36 By S MEHTA
1
 
 

Post A Reply

Temporarily shut down, no new message, sorry.

Name:

Email:



Message:

(Max. 2KB)





Attachment:     (Max. 500kB, .RAR.ZIP.JPG.GIF only)
Verification:

This forum published since July 03, 2002. Renewed on June 22, 2005.

[Plastics Project] [Plastics Machinery] [Plastics Mold] [Discussion Forum] [Contact Kenplas]
Copyright © 2024 Kenplas Industry Limited, Hangzhou Kenplas Machinery Ltd.              Powered by Alentus.