Kenplas Forum ==> Injection Molding (Machine) ==> problems with the filling part.
|
|
|
1 |
hi, in my opinion first increase the water temperature of the mold, increase the peak boost of injection pressure along with shot size.
|
i have problem with the short shots and air entrappment, i'm use a P.B.T resin with 30% glas fiber.
we're fabricating plastic insulator for cars.
some one can help us??
|