2-stage method adopted.
No need to be dried before injection.
Crystallization of preform neck is not needed.
Difficult to be cleaned.
Weak resistance to corrosive detergent.
Can not bear high temperature sterilization.
No action needed to increase its viscosity while recycling. Easy to be recycled.