bir husky hypet 400 makinasında preform üretimi yapıyorum ve oparetörüm sizden istedigim arkadaşlar bu makinayı ögrenmeye başladıgımızda ilk başta nerden ve nasıl başlamalıyız herşeyini tam olarak ögrenmek isitiyorum bilgi verirseniz cok mutlu olurum maillerinizi bekliyorum şimdiden teşekkür ederim

Fine
2
Poor
2012-4-6 1:07:38 By yunus
I'm doing a Husky preform manufacturing machine and oparetörüm hypet 400 friends wanted you to learn this machine and how to start where the first place when we learn to fully hear everything I'll be very happy if you e-mails waiting for information, thank you in advance

Fine
3
Poor
2012-4-6 1:07:10 By yunus
arkadaşlar ben enjeksiyon pet preform işinde çalısıyorum bi senelik deneyımım var ama fazla bir bilgim yok ve amacım herseyini ögrenmek geliştirmek istiyorum kendimi bu alanda yardımcı olursanız çok sevinirim mesala ögrenmek istegim şimdilik basit şeyler ama bana ayrıntılı mal atmak isterseniz cok mutlu olurum mesala siyah leke geliyor preformdan napmalıyız artı baloncuk izleri geliyor babls nasıl gideririz artı vidnın transfer hızını neye göre ayrlıyoruz ve varsa enjeksiyon hakkaında b

Fine
Poor
1
2012-3-24 16:57:25 By yunus
1-reduce nozzle temperature
2-increase holding pressure
3-increase injection time
4-increase cooling time
5-reduce decompression
6-reduce injection speed
7-check dryer

Fine
2
Poor
2012-1-26 18:17:10 By mamdouh elhamalawy
increase hold pressure and increase cooling time.

Fine
1
Poor
2011-6-2 19:04:51 By nvsdrkumar
Dear Sir,
Preform Gate on few particular cavities in a mold not crystalized fully. Due to incmplete crystaliztion centre point appears transperent (amorphous) instead of fully white.
Increasing nozzle tips has not helped much.

Pl guide
Thanks,

Vijay

Fine
3
Poor
2009-1-8 14:56:57 By Vijay

1. Tip temperature too high;
2. Hold pressure/time too low;
3. Mould cooling time too low;
4. Misalignment of HR nozzle and cavity gate.

Fine
12
Poor
2006-2-15 13:54:39 By Kenplas
1
 
 

Post A Reply

Temporarily shut down, no new message, sorry.

Name:

Email:



Message:

(Max. 2KB)





Attachment:     (Max. 500kB, .RAR.ZIP.JPG.GIF only)
Verification:

This forum published since July 03, 2002. Renewed on June 22, 2005.

[Plastics Project] [Plastics Machinery] [Plastics Mold] [Discussion Forum] [Contact Kenplas]
Copyright © 2024 Kenplas Industry Limited, Hangzhou Kenplas Machinery Ltd.              Powered by Alentus.