Why the surface of bottles blown from some preform are smooth but blown from other preforms looks like orange peel (has a lot of small dots, evident more or less)?

Are there any preforms that can not be stretched smoothly in neck zone (the bottles have more or less clear, circular or segmented wave near the support ring or skirt due to sharp change of the wall thickness - above the wave the wall is thick and below — thin)

Is there anywhere illustrated manual of blowing problems/troubleshooting guide?

Fine
6
Poor
4
2009-11-17 5:49:10 By mikhail
1
 
 

Post A Reply

Temporarily shut down, no new message, sorry.

Name:

Email:



Message:

(Max. 2KB)





Attachment:     (Max. 500kB, .RAR.ZIP.JPG.GIF only)
Verification:

This forum published since July 03, 2002. Renewed on June 22, 2005.

[Plastics Project] [Plastics Machinery] [Plastics Mold] [Discussion Forum] [Contact Kenplas]
Copyright © 2024 Kenplas Industry Limited, Hangzhou Kenplas Machinery Ltd.              Powered by Alentus.