Well the gate C.T ( Crystallization) is unavoidable due to hot/cold front.
The body C.T can be reduced by reducing mould temperature (6-8°C is recommended), increase chilled water pressure(6-8 bar) in mould.

Fine
Poor
1
2011-10-27 12:53:16 By tajdar khan
I am molding a large preform. This mold does not have a heated gate area. I am having a white ring around the sprue area and the bottle is hazzy when fully packed out. If underpacked bottle looks clear, However it is still white at gate area. Any suggestions?

Fine
10
Poor
2011-8-5 20:12:33 By Danny
1
 
 

Post A Reply

Temporarily shut down, no new message, sorry.

Name:

Email:



Message:

(Max. 2KB)





Attachment:     (Max. 500kB, .RAR.ZIP.JPG.GIF only)
Verification:

This forum published since July 03, 2002. Renewed on June 22, 2005.

[Plastics Project] [Plastics Machinery] [Plastics Mold] [Discussion Forum] [Contact Kenplas]
Copyright © 2025 Kenplas Industry Limited, Hangzhou Kenplas Machinery Ltd.              Powered by Alentus.