1. Reduce barrel temperature;
2. Reduce Injection speed (increase injection time);
3. Increase Hold-pressure time;
4. Decompression time too high;
5. Mould cooling time too low;
6. Poor mould cooling. Check molding cooling, core temperature;
7. Water leakage in mold cavities.